Chart
Block Printing Ink Drying Times by Ink Type
Published Updated
As an Amazon Associate we earn from qualifying purchases. This does not change our picks. Affiliate disclosure
Short answer
Water based block printing ink dries fastest: Essdee gives about 2 hours on a rack in a warm, dry room and up to weeks in a cold studio. Oil based ink takes days, and Cranfield and Speedball state no fixed time for paper. On fabric, Speedball fabric ink is dry to the touch overnight and Gamblin gives 3 to 7 days for its relief ink.
Gear for this job
All 7 picks comparedSpeedball water-soluble ink set, 6 x 1.25 fl oz
See price on AmazonSee it on AmazonSpeedball water-soluble block ink, black, 8 fl oz
See price on AmazonSee it on AmazonHandy Art water-soluble block ink, black, 16 oz
See price on AmazonSee it on Amazon

The honest answer is a range, because the room matters as much as the ink. This chart lists what each maker states about its own ink, with the ink named. Where a maker's page gives no figure, the cell says so and nothing is guessed. Use it to decide when lino prints can be stacked, framed or mailed, and when printed fabric can be washed. Dry to the touch is not the same as dry all the way through, so the sections under the chart explain how to check a print and what slows drying down.
Block printing ink drying time chart
Times assume a thin, even ink film. The third column is the maker's own statement about drying. The fourth column applies only to prints on fabric. Where it says no figure, read the label of the ink you bought.
| Ink type | Ink | Drying, as the maker states it | Fabric: before washing |
|---|---|---|---|
| Water based | Essdee block printing ink | About 2 hours on a rack in a warm, dry room. Could take weeks in a cold studio | Not for fabric |
| Water based | Speedball Water-Soluble Block Printing Ink | No figure on the product page | Not for fabric |
| Water-washable oil | Cranfield Caligo Safe Wash Relief Ink | No fixed time for paper. Depends on conditions: allow days | Several days as a guide. 7 days in the maker's wash test |
| Water-washable oil | Speedball Professional Relief Ink | No figure on the product page. Allow days | No figure |
| Oil based | Speedball Oil-Based Relief Ink | No figure on the product page. Allow days | No figure |
| Oil based | Gamblin Relief Ink | No figure for paper on the maker's page | Dry in 3 to 7 days, then 1 to 2 more weeks to cure. No heat set |
| Fabric ink, oil base | Speedball Fabric Block Printing Ink | Dry to the touch overnight. No heat set required | No maker figure. Listings say about a week |
| Fabric ink, water based | Essdee fabric block printing ink | No figure. Dries, then must be heat set | After heat setting, as the label says |
| Acrylic plus medium | Daler-Rowney System3 Block Printing Medium | Dries fast. No maker figure | Not stated |
How long should I let ink dry before stacking or mailing?
Go by a test, not the clock. Rub a solid area of a spare print gently with a clean fingertip. If no color comes off and the surface is not tacky, the print can be handled. Cranfield describes the same gentle rub test in its fabric guide. Until then, keep prints apart, flat or hanging, with air on both sides.
Stacking, framing under glass and mailing all press something against the ink, so they need a print that passes the rub test on its thickest area, not just its edges. Water based block ink has one more limit: it stays water-soluble when dry, so a damp hand can still smudge a print that passed the test.
Ink drying time: water based vs oil based block printing ink
Water based block printing ink dries as its water leaves into the paper and the air. That is fast in a warm, dry room, which is how Essdee arrives at about 2 hours, and slow in a cold or humid one. Oil based block printing ink does not dry by evaporation. The oil hardens as it reacts with air, which takes days and goes on after the surface feels dry. That is why Cranfield lists warm air, low humidity, airflow and light as the things that speed it up, and gives no number of hours.
Water-washable oil inks such as Caligo Safe Wash and Speedball Professional Relief Ink are oil inks in this respect. They wash up with soap, but they dry like oil. The trade-offs are set out in oil based vs water based ink.
What slows block printing ink down
Essdee and Cranfield name the same causes. Most of them are in your hands before the print is pulled, and the first one matters most.
- A thick ink film. Essdee says thinner layers dry faster. Roll the ink out thin, as in how to use a brayer.
- A cold room. Both makers put warmth first. Essdee's weeks figure is for a cold studio.
- Humid air. Cranfield lists low relative humidity among the main things that promote drying.
- No airflow. Prints in a closed stack or a still corner dry slowly. A rack or a line lets air reach each sheet.
- Paper that does not absorb. Essdee advises absorbent, matte paper. Cranfield adds that paper sizing, absorbency and acidic papers all change the time.
Block printing ink for fabric: how long before washing?
Fabric has two waits: dry to the touch, then ready to wash. Speedball says its fabric ink dries to the touch overnight and needs no heat set, but its product page gives no wait before washing. Retail listings and a supplier tutorial say about a week. Essdee's fabric ink works the other way: it bonds once it has dried and been heat set, as the label describes.
Oil inks on fabric take longest. Cranfield says Safe Wash is made for paper, dries slower than fabric ink and should dry for several days before handling or washing, with 7 days in its own wash test. Gamblin gives 3 to 7 days to dry plus a week or two before laundering, and says not to heat set. No maker promises that a print survives washing. Steps are in how to block print on fabric.
Note.Heat rules differ by maker: Essdee fabric ink must be heat set, Speedball fabric ink needs none, and Gamblin says do not heat set. Follow the label of your ink, not a general rule.
What to do with a print that stays tacky
The usual causes of a tacky print are the ones in the list above: a thick ink film, a cool room or damp air. Change the conditions first, then give it time.
- 1
Separate the prints. Lay each one flat on its own or hang it, so air reaches the whole inked surface. Never leave tacky prints stacked.
- 2
Move them to the warmest, driest room you have, with moving air. For oil based ink, Cranfield also lists exposure to light as a help.
- 3
Test again the next day with a gentle rub on a spare print. Oil based ink can need several more days, so keep testing before you stack or frame.
- 4
For the next batch, roll a thinner film and choose absorbent, matte paper. Thin ink that hisses lightly under the brayer dries far sooner than a thick, glossy layer.
- 5
With oil based ink, a drier is the maker's own remedy. Cranfield sells a wax drier for its inks, and its fabric guide mentions adding a drop of cobalt or manganese drier. Follow the drier's instructions.
Which ink should you buy?
The chart shows the trade: water based ink dries as its water leaves into the paper and the air, which is quick in a warm, dry room, while oil based ink stays workable longer and takes longer to dry. If you want prints you can stack and mail sooner, start with water based ink. Our water based ink guide compares inks and sets by volume, number of colors and cleanup.
Quick answers
Short answers, each from the maker of the ink named. If the label on your tube says something different, the label wins.
- How long does water based block printing ink take to dry? Essdee gives about 2 hours on a rack in a warm, dry room and up to weeks in a cold studio. Speedball states no figure.
- How long does oil based block printing ink take to dry? Days. Cranfield and Speedball give no fixed time for paper, because warmth, humidity, airflow and ink thickness decide it.
- How long before block printing ink for fabric can be washed? Speedball fabric ink: listings say about a week. Gamblin relief ink: 3 to 7 days to dry, then 1 to 2 weeks more.
- How long should I let ink dry before framing? Until a solid area passes a gentle rub test with no color on the finger and no tack. For oil based ink that means days.
- Does acrylic paint with block printing medium dry faster? Yes, it dries fast, on the block as well. See acrylic paint for block printing.
Use this chart
Print it, save the image version, or put it on your own site or forum post with the code below. The code keeps a link back to this page as the source.
Embed code
<a href="https://inkedblock.com/blog/block-printing-ink-drying-time"><img src="https://inkedblock.com/charts/block-printing-ink-drying-time/image.png" alt="Block Printing Ink Drying Times by Ink Type" width="600" loading="lazy"></a> <p>Source: <a href="https://inkedblock.com/blog/block-printing-ink-drying-time">Block Printing Ink Drying Times by Ink Type</a>, Inked Block</p>
What you need for this
- See price on AmazonAmazon
Speedball water-soluble ink set, 6 x 1.25 fl oz
- See price on AmazonAmazon
Caligo Safe Wash relief ink, black, 75 ml
From Best Oil Based Block Printing Inks, Including Water-Washable
- See price on AmazonAmazon